Currently I am simulating the part distortion after it is ejected from Die in High pressure die casting. I had conducted this simulation in two steps(explicit), For initial study Die is considered as rigid body,
Simulation:
Step1: Initial condition for temperatures of part is given and in step-1, final temp of the part is defined and general contact is modeled between part and die, Due to temperature difference part is shrinking and catching the die.Time i had given as 0.1 sec(assumption). this is done steady state.
Step2: velocity(assumption=300mm/sec) is given at ejection location on the part to overcome the contact pressure established in step-1
Then checking the PEEQ for the part
Is this approach makes sense? Only reason why I am not doing this implicit is due to stability issues and convergence.
But not sure this can be done in explicit especially step-1.
Can someone help me?