LaRC05 failure criterion

Has damage evolution for the LaRC05 failure criterion been implemented? I was able to get everything to work without the *damage evolution keyword, but I run into issues once I incorporate the damage evolution keyword. I also saw that it appears that it is reading the *shell section card twice. I am only defining the shell section once within the input file.

I am using S4 elements. The version of Abaqus that I am using is Abaqus 2023.HF2

Material input: 

*Material, name=mat
*Damage Initiation, criterion=LARC05
261925., 208524., 16721., 25075., 11799., 0.925025, 0.0569725, 11799.
0.082, 0.28
*Damage Evolution, type=ENERGY, softening=LINEAR
81.5, 106.3, 0.277, 0.788
*Density
6.22e-05,
*Elastic, type=LAMINA
2.28e+07, 1.3e+06, 0.32, 737000., 737000., 435000.

Error:

***ERROR: A MATERIAL PROPERTY HAS BEEN DEFINED MORE THAN ONCE FOR THIS MATERIAL
***NOTE: DUE TO AN INPUT ERROR THE ANALYSIS PRE-PROCESSOR HAS BEEN UNABLE TO 
INTERPRET SOME DATA. SUBSEQUENT ERRORS MAY BE CAUSED BY THIS OMISSION
*Orientation, name=Part-1-1-Ori-1
*Shell Section, elset=Part-1-1_Set-3, material=IM7_8552, orientation=Part-1-1-Ori-1
*Shell Section, elset=Part-1-1_Set-3, material=IM7_8552, orientation=Part-1-1-Ori-1

***ERROR: THERE IS NO MATERIAL BY THE NAME IM7_8552